This product's A and B components are both packaged in plastic drums.
Component A: 20kg/drum Component B: 10kg/drum
Testing Items | Testing Conditions | QUALIFICATION INDEX (GB50728-2011) |
|
---|---|---|---|
Colloidal Properties | Tensile strength (MPa) | Under conditions of (23±2)°C and (50±5)% relative humidity, the test is conducted at a loading rate of 2mm/min. | ≥30 |
Tensile modulus of elasticity (MPa) | ≥1.5×10³ | ||
Elongation (100%) | ≥1.5 | ||
Flexural strength (MPa) | ≥40, and no fracture failure is allowed | ||
Compressive strength (MPa) | ≥70 | ||
Adhesive Capability |
Standard value of steel-to-steel tensile shear strength (MPa) | (23±2)℃, (50±5) %RH | ≥10 |
Steel-to-steel bond tensile strength (MPa) | At (23±2)°C and (50±5)% RH, the test is conducted according to the specified loading speed as per the test method standard. | ≥32 | |
Steel-to-steel T-peel adhesion length (mm) | ≤35 | ||
Steel-to-C45 tensile bond strength (MPa) | ≥2.5, and cohesive failure within the concrete | ||
Thermal deformation temperature (℃) | Method B of 0.45MPa bending stress was used | ≥60 | |
Non-volatile matter content (%) | (105±2)℃, (180±5) min | ≥99 |